Grade St13
Germany W-Nr. 1.0347
Corresponding Standard DIN 1623-1-1983
Cold rolled strip and sheet – Technical delivery conditions – General structural steels
Classification Carbon Steel
St13 Chemical Element Composition Content (%)
Component C Al
Minimum Value - 0.02
Maximum Value 0.1 -
St13 Mechanical Properties
condition Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Thin plate, Coil; Cold rolled 270~370 ≤240 ≥34 HRB
≤55
Approximate Comparison Table
Japan Germany France European Standard Russia Sweden United Kingdom
JIS DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS
SPCD St13
USt14
1.0336 E DC03
FeP03①
1.0347 08YU 1146 CR2
CR3
St13 Corresponding Standards(Same grade name, different standards)