USA UNS N08028
Corresponding Standard ASTM A213/A213M-2019
Seamless Ferritic and Austenitic Alloy-Steel Boiler, Superheater, and Heat-Exchanger Tubes
Classification Austenitic Stainless Steel
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo
Minimum Value - - - - - 26 30 0.6 3
Maximum Value 0.03 1 2.5 0.03 0.03 28 34 1.4 4
Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
≥500 ≥214 ≥40
1 Approximate Comparison Table Corrosion-Resistant Alloy
China United States Germany
GB ISC UNS DIN EN/DIN W-Nr.
NS 1404
BG2830
H 08028 N 08028
Sanicro 28
X1NiCrMoCu 31-27-4 1.4563
2 Approximate Comparison Table Austenitic Stainless Steel
United States International Organization for Standardization European Standard
UNS ISO Numerical Grade EN Numerical Grade
N08028 X1NiCrMoCu31-27-4 4563-080-28-I X1NiCrMoCu31-27-4 1.4563

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!