Grade A249 TP347H
USA UNS S34709
Corresponding Standard ASTM A249/A249M-2004
Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes
Classification Austenitic Stainless Steel
A249 TP347H Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni More
Minimum Value 0.04 - - - - 17 9 Nb(Cb):8C~1.10
Maximum Value 0.1 1 2 0.045 0.03 19 12
A249 TP347H Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
≥515 ≥205 ≥35 HRB
≤90
Approximate Comparison Table Austenitic Stainless Steel
China Japan United States International Organization for Standardization France European Standard
GB ISC JIS ASTM/AISI UNS ISO Numerical Grade NF EN/NF EN Numerical Grade
07Cr18Ni11Nb
(1Cr19Ni11Nb)
S34779 SUS347H 347H S34709 X7CrNiNb18-10 4912-347-09-I Z2CND17-11
Z2CND18-13
Z8CNNb18-10
X7CrNiNb18-10 1.4912
A249TP347H Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!