USA UNS S44625
Corresponding Standard ASTM A493-2016
Standard Specification for Stainless Steel Wire and Wire Rods for Cold Heading and Cold Forging
Classification Ferritic Stainless Steel
Properties Corrosion Resistance Good Forgability
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo N More
Minimum Value - - - - - 25 - - 0.75 - Ni+Cu≤0.5
Maximum Value 0.01 0.4 0.4 0.02 0.02 27.5 0.5 0.2 1.5 0.15
Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Wires, rebar; d≥2.5 Annealing ≤690
Wires, rebar; d≥2.5 Light Drawing ≤725
Approximate Comparison Table Ferritic Stainless Steel
China Taiwan, China Japan South Korea United States Germany France
GB ISC CNS JIS KS ASTM UNS DIN EN/DIN W-Nr. NF EN/NF
008Cr27Mo
(00Cr27Mo)
S12791 XM27 SUS XM27 STS XM27 XM27 S44625 X1CrMo 26-1 1.4131 Z01CD 26-1