USA UNS S42010
Corresponding Standard ASTM A493-2016
Standard Specification for Stainless Steel Wire and Wire Rods for Cold Heading and Cold Forging
Classification Martensitic Stainless Steel
Properties Corrosion Resistance Good Forgability
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo
Minimum Value 0.15 - - - - 13.5 0.35 0.4
Maximum Value 0.3 1 1 0.04 0.03 15 0.85 0.85
Mechanical Properties
diameter
d
mm
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Wires, rebar; d≥2.5 Annealing ≤690
Wires, rebar; d≥2.5 Light Drawing ≤725
Approximate Comparison Table Martensitic Heat-Resistant Steel
China Japan United States Germany France European Standard Russia Sweden United Kingdom
GB JIS ASTM UNS DIN EN/DIN NF EN/NF EN Numerical Grade GOST SS BS EN/BS
20Cr13
2Cr13
X20Cr13
SUS420J1 420 S42010
S42010
X20Cr13 X20Cr13
Z20C13
X20Cr13 1.4021 20KH13 2303 420S29
420S37