Grade SNB16
Corresponding Standard JIS G 4107-2007
Alloy Steel Bolting Materials for High Temperature Service
Classification Alloy Steel
SNB16 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Mo V
Minimum Value 0.36 0.2 0.45 - - 0.8 0.5 0.25
Maximum Value 0.44 0.35 0.7 0.04 0.04 1.15 0.65 0.35
SNB16 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Bar, Wire, Bolt; d≤63 Normalizing + Tempering or Quenching + Tempering ≥860 ≥725 ≥18 ≥50
Bar, Wire, Bolt; 63<d≤100 Normalizing + Tempering or Quenching + Tempering ≥760 ≥655 ≥17 ≥50
Bar, Wire, Bolt; 100<d≤120 Normalizing + Tempering or Quenching + Tempering ≥690 ≥590 ≥16 ≥50
Approximate Comparison Table Structural Alloy Steel
China Japan United States Germany European Standard United Kingdom
GB JIS ASTM DIN EN/DIN W-Nr. EN Numerical Grade BS EN/BS
35CrMoV SNB16 A193 B16 40CrMoV4-6 1.7711 40CrMoV4-6 1.7711 40CrMoV4-6