Grade Type 405
USA UNS S40500
Corresponding Standard ASTM A580/A580M-2018
Stainless Steel Wire
Classification Ferritic Stainless Steel
Type 405 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Al
Minimum Value - - - - - 11.5 0.1
Maximum Value 0.08 1 1 0.04 0.03 14.5 0.3
Type 405 Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
A Cold Precision Rolling ≥485 ≥275 ≥16 ≥45
A Annealing ≥485 ≥275 ≥20 ≥45
1 Approximate Comparison Table Ferritic Stainless Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Sweden United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade SS BS EN/BS
06Cr13Al S11348 405 SUS 405 STS 405 405 S40500 X6CrAl 13 X6CrAl 13
(X7CrAl 13)
1.4002 Z6CA 13 X6CrAl 13 1.4002 2302 405S17
2 Approximate Comparison Table Ferritic Heat-Resistant Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS
06Cr13Al
(0Cr13Al)
S11348 405 SUS 405 STR 405 405 S40500 X6CrAl 13
2
ISO 683-13-1986
X6CrAl 13
(X7CrAl 13)
1.4002 Z6CA 13 X6CrAl 13 1.4002 1Х20Ю 2302 405S17

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!