Grade Type 414
USA UNS S41400
Corresponding Standard ASTM A580/A580M-2018
Stainless Steel Wire
Classification Martensitic Stainless Steel
Type 414 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value - - - - - 11.5 1.25
Maximum Value 0.15 1 1 0.04 0.03 13.5 2.5
Type 414 Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Hardness
HBW
A Cold Precision Rolling ≤1035
t≤9.5mm 955°C, Oil Cooling HRC
≥42