Grade SUS403
Other Names
Corresponding Standard JIS G 4311-2019
Heat-resisting steel bars and wire rods
Classification Martensitic Stainless Steel
Properties Corrosion Resistance
Density 7.75 g/cm3
SUS403 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value - - - - - 11.5 -
Maximum Value 0.15 0.5 1 0.04 0.03 13 0.6
SUS403 Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
Quenching + Tempering ≥590 ≥390 ≥25 ≥55 ≥170 ≥147
Approximate Comparison Table
China Taiwan, China Japan South Korea United States Russia Sweden United Kingdom
GB ISC CNS JIS KS ASTM UNS GOST SS BS EN/BS
12Cr12
(1Cr12)
S40310 403 SUS 403 STS 403 403 S40300 08Х13 2301 403S17

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!