Grade SUS310S-HR
Corresponding Standard JIS G 4311-2019
Heat-resisting steel bars and wire rods
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
Density 7.98 g/cm3
SUS310S-HR Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value - - - - - 24 19
Maximum Value 0.08 1.5 2 0.045 0.03 26 22
SUS310S-HR Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Solution Heat Treatment (S) ≥520 ≥205 ≥40 ≥50 ≤187
SUS310S-HR Corresponding Standards(Same grade name, different standards)