Grade TP 304LN
USA UNS S30453
Corresponding Standard ASTM A376/A376M-2019
Seamless Austenitic Steel Pipe for High-Temperature Service
Classification Austenitic Stainless Steel
TP 304LN Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni N
Minimum Value - - - - - 18 8 0.1
Maximum Value 0.035 0.75 2 0.045 0.03 20 11 0.16
TP 304LN Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
≥515 ≥205 (Longitudinal 35, Transverse 25), min
Approximate Comparison Table Austenitic Stainless Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Sweden United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade SS BS EN/BS
022Cr19Ni10N
(00Cr18Ni10N)
S30453 304LN SUS 304LN STS 304LN 304LN S30453 X2CrNiN 18-9
X2CrNiN18-10
X2CrNiN 18-10 1.4311 Z2CN 18-1Az
Z3CN18-10Az
X2CrNiN 18-10 1.4311 2371 304S62