USA UNS S30300
AISI
American Iron and Steel Institute
303
Corresponding Standard ASTM A582/A582M-2012(R2017)
Free-Machining Stainless Steel Bars
Classification Austenitic Stainless Steel
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value - - - - 0.15 17 8
Maximum Value 0.15 1 2 0.2 - 19 10
Mechanical Properties
Heat Treatment or Condition
Hardness
HBW
Annealing ≤262
Approximate Comparison Table Austenitic Stainless Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO Numerical Grade DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade BS EN/BS
Y12Cr18Ni9
(Y1Cr18Ni9)
S30317 303 SUS 303 STS 303 303 S30300 X10CrNiS 18-9 4305-303-00-I X8CrNiS 18-9
(X10CrNiS 18-9)
1.4305 Z10CNF 18-09 X8CrNiS 18-9 1.4305 303S21

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!