USA UNS S41041
Corresponding Standard ASTM A565/A565M-2010(R2017)
Martensitic Stainless Steel Bars for High-Temperature Service
Classification Martensitic Stainless Steel
Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo Nb Al
Minimum Value 0.13 - 0.4 - - 11.5 - - 0.15 -
Maximum Value 0.18 0.5 0.6 0.03 0.03 13 0.5 0.2 0.45 0.05
Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
≥795 ≥515 ≥15 ≥50 ≤277 ≥27