Grade A249 TP201
USA UNS S20100
Corresponding Standard ASTM A249/A249M-2018
Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes
Classification Austenitic Stainless Steel
A249 TP201 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni N
Minimum Value - - 5.5 - - 16 3.5 -
Maximum Value 0.15 1 7.5 0.06 0.03 18 5.5 0.25
A249 TP201 Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Solutioning Temperature 1040℃ ≥655 ≥260 ≥35 HRB
≤95
1 Approximate Comparison Table
China Taiwan, China Japan South Korea United States International Organization for Standardization European Standard
GB ISC CNS JIS KS ASTM UNS ISO EN Numerical Grade
12Cr17Mn6Ni5N
(1Cr17Mn6Ni5N)
S35350 201 SUS 201 STS 201 201 S20100 X12CrMnNi 17-7-5
X9CrMnNiCu17-8-5-2
X12CrMnNi 17-7-5
X9CrMnNiCu17-8-5-2
1.4372
1.4618
2 Approximate Comparison Table
China Japan United States International Organization for Standardization European Standard
ISC JIS UNS ISO Numerical Grade Numerical Grade
S35350 SUS201 S20100 X12CrMnNiN17-7-5 4372-201-00-I 1.4372
A249TP201 Corresponding Standards(Same grade name, different standards)