Grade A249 TP304
USA UNS S30400
Corresponding Standard ASTM A249/A249M-2018
Welded Austenitic Steel Boiler, Superheater, Heat-Exchanger, and Condenser Tubes
Classification Austenitic Stainless Steel
A249 TP304 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni
Minimum Value - - - - - 18 8
Maximum Value 0.08 1 2 0.045 0.03 20 11
A249 TP304 Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Solutioning Temperature 1040℃ ≥515 ≥205 ≥35 HRB
≤90
1 Approximate Comparison Table Austenitic Stainless Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO Numerical Grade DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS
06Cr19Ni9 S30408 304 SUS 304 STS 304 304 S30400 X5CrNi 18-10 4301-304-00-I X5CrNi 18-10
(X5CrNi 18-9)
1.4301 Z6CN 18-09 X5CrNi 18-10 1.4301 08Х18Н10 2332
2333
304S15
2 Approximate Comparison Table Austenitic Heat-Resistant Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS
06Cr19Ni10
(0Cr18Ni9)
S30408 304 SUS 304 STS 304 304 S30400 X5CrNi 18-10 X5CrNi 18-10
(X5CrNi 18-9)
1.4301 Z6CN 18-09 X5CrNi 18-10 1.4301 08Х18Н10 2332
2333
304S15
3 Approximate Comparison Table Stainless Steels for Cold Heading and Cold Extruding
China Japan United States International Organization for Standardization European Standard
GB ISC JIS ASTM/AISI UNS ISO Numerical Grade EN Numerical Grade
06Cr19Ni10
(0Cr18Ni9)
S30408 SUS304 304 S30400 X5CrNi18-10 4301-304-00-I X5CrNi18-10 1.4301
A249TP304 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!