Grade C25
Corresponding Standard ISO 683-1-2016
Non-alloy steels for quenching and tempering
Classification Carbon Steel
C25 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo More
Minimum Value 0.22 0.1 0.4 - - - - - - Cr+Mo+Ni≤0.63
Maximum Value 0.29 0.4 0.7 0.045 0.045 0.4 0.4 0.3 0.1
C25 Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
d≤16 or t≤8 550~700 ≥370 ≥19
16<d≤40 or 8<t≤20 500~650 ≥320 ≥21
1 Approximate Comparison Table Carbon Structural Steel and Engineering Steel
China Japan International Organization for Standardization
GB JIS ISO
25 S25C C25
2 Approximate Comparison Table High-Quality Carbon Structural Steel
China Japan United States International Organization for Standardization Germany European Standard Russia Sweden United Kingdom
GB JIS SAE ISO DIN EN/DIN W-Nr. EN Numerical Grade GOST SS BS EN/BS
20 S20C
S22C
1020 C25 C22 1.0402 C22 1.0402 20 1450 070M20
3 Approximate Comparison Table Carbon Structural Steel and Engineering Steel
International Organization for Standardization Germany European Standard Russia
ISO DIN EN/DIN EN Numerical Grade GOST
C25 C25 C25 1.0406 25
4 Approximate Comparison Table High-Quality Carbon Structural Steel
China Japan United States International Organization for Standardization France Russia United Kingdom
GB JIS ASTM/AISI ISO NF EN/NF GOST BS EN/BS
GB/T 699-1999
25
S25C 1025 ISO 630-1:1987
C25
C25E4
C25M2
C25
XC25
25 060A25
070A26
C25 Corresponding Standards(Same grade name, different standards)