Grade C35E
Corresponding Standard ISO 683-1-2016
Non-Alloy Steels for Quenching and Tempering
Classification Carbon Steel
C35E Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo More
Minimum Value 0.32 0.1 0.5 - - - - - - Cr+Mo+Ni≤0.63
Maximum Value 0.39 0.4 0.8 0.025 0.035 0.4 0.4 0.3 0.1
C35E Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Impact Energy Absorption
KV2
J
d≤16 or t≤8 630~780 ≥430 ≥17 ≥40 ≥25
16<d≤40 or 8<t≤20 600~750 ≥380 ≥19 ≥45 ≥25
40<d≤100 or 20<t≤60 550~700 ≥320 ≥20 ≥50 ≥25
Approximate Comparison Table Non-Alloy Steel for Quenching and Tempering
China Japan International Organization for Standardization European Standard
GB JIS ISO EN Numerical Grade
35 S35C C35E C35E 1.1181