Grade C35EC
Germany W-Nr. 1.1172
Old Grade
Corresponding Standard DIN EN 10263-4-2018
Steel rod, bars and wire for cold heading and cold extrusion Part 4: Technical delivery conditions for steels for quenching and tempering
Classification Carbon Steel
Properties Forgability
C35EC Chemical Element Composition Content (%)
Component C Si Mn P S Cu
Minimum Value 0.32 - 0.5 - - -
Maximum Value 0.39 0.3 0.8 0.025 0.025 0.25
C35EC Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Reduction of Area
ψ
%
Bars, wires; 2<d≤5 Untreated, Cold Drawn, Spheroidizing Treatment (+U+C+AC) ≤550 ≥62
Bars, wires; 5<d≤40 Untreated, Cold Drawn, Spheroidizing Treatment (+U+C+AC) ≤540 ≥62
Bars, wires; 2<d≤5 Untreated and Cold Drawn and Spheroidizing Treatment and Quenching Rolling (+U+C+AC+LC) ≤590 ≥60
Bars, wires; 5<d≤40 Untreated and Cold Drawn and Spheroidizing Treatment and Quenching Rolling (+U+C+AC+LC) ≤580 ≥60
Bar stock, rod stock; 5<d≤40 Spheroidizing or Spheroidizing + Rotary Peeling (+AC or +AC+PE) ≤560 ≥60
Bar, Wire; 5<d≤10 Spheroidizing Treatment and Cold Drawing (+AC+C) ≤670
Bar, Wire; 10<d≤40 Spheroidizing Treatment and Cold Drawing (+AC+C) ≤660
New and Old Grade Replacement List
Approximate Comparison Table
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France Russia United Kingdom
GB ISC CNS JIS KS ASTM/AISI UNS ISO DIN EN/DIN W-Nr. NF EN/NF GOST BS EN/BS
ML35 U40352 SWRCH35K SWRCH35K SWRCH35K 1034 G10340 CE35E4
(C3)
Cq35
(C35C)
1.1172 XC38
FR36
35 1/2