Grade
C35RC
Germany W-Nr.
1.1060
Corresponding Standard
DIN EN 10263-4-2018
Steel Rod, Bars and Wire for Cold Heading and Cold Extrusion Part 4: Technical Delivery Conditions for Steels for Quenching and Tempering
Classification
Carbon Steel
Properties
Forgability
C35RC Chemical Element Composition Content (%)
Component
C ⓓ
Si ⓔ
Mn
P
S
Cu
Minimum Value
0.32
-
0.5
-
0.02
-
Maximum Value
0.39
0.3
0.8
0.025
0.035
0.25
C35RC Mechanical Properties
condition
Heat Treatment or Condition
Tensile Strength σb
Mpa
Reduction of Area ψ
%
Bars, wires; 2<d≤5
Untreated, Cold Drawn, Spheroidizing Treatment (+U+C+AC)
≤550
≥62
Bars, wires; 5<d≤40
Untreated, Cold Drawn, Spheroidizing Treatment (+U+C+AC)
≤540
≥62
Bars, wires; 2<d≤5
Untreated and Cold Drawn and Spheroidizing Treatment and Quenching Rolling (+U+C+AC+LC)
≤590
≥60
Bars, wires; 5<d≤40
Untreated and Cold Drawn and Spheroidizing Treatment and Quenching Rolling (+U+C+AC+LC)
≤580
≥60
Bar stock, rod stock; 5<d≤40
Spheroidizing or Spheroidizing + Rotary Peeling (+AC or +AC+PE)
≤560
≥60
Bar, Wire; 5<d≤10
Spheroidizing Treatment and Cold Drawing (+AC+C)
≤670
Bar, Wire; 10<d≤40
Spheroidizing Treatment and Cold Drawing (+AC+C)
≤660
C35RC Corresponding Standards(Same grade name, different standards)
Message
I want to correct it
Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!