Grade
38Cr2
Germany W-Nr.
1.7003
Corresponding Standard
DIN EN 10263-4-2018
Steel rod, bars and wire for cold heading and cold extrusion Part 4: Technical delivery conditions for steels for quenching and tempering
Classification
Alloy Steel
38Cr2 Chemical Element Composition Content (%)
Component
C ⓓ
Si ⓔ
Mn
P
S
Cr
Cu
Minimum Value
0.35
-
0.5
-
-
0.4
-
Maximum Value
0.42
0.3
0.8
0.025
0.025
0.6
0.25
38Cr2 Mechanical Properties
condition
Heat Treatment or Condition
Tensile Strength σb
Mpa
Reduction of Area ψ
%
Wire; 2<d≤5
Spheroidizing + Cold Drawn + Spheroidizing (+AC+C+AC)
≤590
≥62
Wire; 5<d≤40
Spheroidizing + Cold Drawn + Spheroidizing (+AC+C+AC)
≤580
≥62
Bars, wires; 2<d≤5
Spheroidizing + Cold Drawn + Spheroidizing + Quenched Rolling (+AC+C+AC+LC)
≤630
≥60
Bars, wires; 5<d≤40
Spheroidizing + Cold Drawn + Spheroidizing + Quenched Rolling (+AC+C+AC+LC)
≤620
≥60
Bars, rods, wires; 5<d≤40
Spheroidizing or Spheroidizing + Rotary Peeling (+AC or +AC+PE)
≤600
≥60
Approximate Comparison Table structural alloy steel
38Cr2 Corresponding Standards(Same grade name, different standards)
Message
I want to correct it
Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!