Grade 46Cr2
Germany W-Nr. 1.7006
Corresponding Standard DIN EN 10263-4-2018
Steel rod, bars and wire for cold heading and cold extrusion Part 4: Technical delivery conditions for steels for quenching and tempering
Classification Alloy Steel
46Cr2 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Cu
Minimum Value 0.42 - 0.5 - - 0.4 -
Maximum Value 0.5 0.3 0.8 0.025 0.025 0.6 0.25
46Cr2 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Reduction of Area
ψ
%
Wire; 2<d≤5 Spheroidizing + Cold Drawn + Spheroidizing (+AC+C+AC) ≤610 ≥60
Wire; 5<d≤40 Spheroidizing + Cold Drawn + Spheroidizing (+AC+C+AC) ≤600 ≥60
Bars, wires; 2<d≤5 Spheroidizing + Cold Drawn + Spheroidizing + Quenched Rolling (+AC+C+AC+LC) ≤650 ≥58
Bars, wires; 5<d≤40 Spheroidizing + Cold Drawn + Spheroidizing + Quenched Rolling (+AC+C+AC+LC) ≤640 ≥58
Bars, rods, wires; 5<d≤40 Spheroidizing or Spheroidizing + Rotary Peeling (+AC or +AC+PE) ≤620 ≥58
1 Approximate Comparison Table Structural Alloy Steel
Germany European Standard
DIN EN/DIN W-Nr. EN Numerical Grade
46Cr2 1.7006 46Cr2 1.7006
2 Approximate Comparison Table Structural Alloy Steel
China International Organization for Standardization Germany European Standard
GB ISO DIN EN/DIN EN
45Cr 46Cr2 46Cr2 46Cr2

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!