Grade 37Cr4
Germany W-Nr. 1.7034
Corresponding Standard DIN EN 10263-4-2018
Steel rod, bars and wire for cold heading and cold extrusion Part 4: Technical delivery conditions for steels for quenching and tempering
Classification Alloy Steel
37Cr4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Cu
Minimum Value 0.34 - 0.6 - - 0.9 -
Maximum Value 0.41 0.3 0.9 0.025 0.025 1.2 0.25
37Cr4 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Reduction of Area
ψ
%
Wire; 2<d≤5 Spheroidizing + Cold Drawn + Spheroidizing (+AC+C+AC) ≤580 ≥62
Wire; 5<d≤40 Spheroidizing + Cold Drawn + Spheroidizing (+AC+C+AC) ≤570 ≥62
Bars, wires; 2<d≤5 Spheroidizing + Cold Drawn + Spheroidizing + Quenched Rolling (+AC+C+AC+LC) ≤620 ≥60
Bars, wires; 5<d≤40 Spheroidizing + Cold Drawn + Spheroidizing + Quenched Rolling (+AC+C+AC+LC) ≤610 ≥60
Bars, rods, wires; 5<d≤40 Spheroidizing or Spheroidizing + Rotary Peeling (+AC or +AC+PE) ≤590 ≥60
Approximate Comparison Table structural alloy steel
China Japan United States International Organization for Standardization Germany France European Standard Russia Sweden United Kingdom
GB JIS ASTM ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST SS BS EN/BS
35Cr SCr435H Gr.5135 37Cr4 37Cr4 1.7034 37Cr4
38C4
37Cr4 1.7034 38KHA
40KH
2245 530A36
530M36

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!