Grade 37CrMo4
Germany W-Nr. 1.7202
Corresponding Standard DIN EN 10263-4-2018
Steel rod, bars and wire for cold heading and cold extrusion Part 4: Technical delivery conditions for steels for quenching and tempering
Classification Alloy Steel
37CrMo4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Cu Mo
Minimum Value 0.35 - 0.6 - - 0.9 - 0.15
Maximum Value 0.4 0.3 0.9 0.025 0.025 1.2 0.25 0.3
37CrMo4 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Reduction of Area
ψ
%
Wire; 2<d≤5 Spheroidizing + Cold Drawn + Spheroidizing (+AC+C+AC) ≤610 ≥62
Wire; 5<d≤40 Spheroidizing + Cold Drawn + Spheroidizing (+AC+C+AC) ≤600 ≥62
Bars, wires; 2<d≤5 Spheroidizing + Cold Drawn + Spheroidizing + Quenched Rolling (+AC+C+AC+LC) ≤650 ≥60
Bars, wires; 5<d≤40 Spheroidizing + Cold Drawn + Spheroidizing + Quenched Rolling (+AC+C+AC+LC) ≤640 ≥60
Bars, rods, wires; 5<d≤40 Spheroidizing or Spheroidizing + Rotary Peeling (+AC or +AC+PE) ≤620 ≥60
37CrMo4 Corresponding Standards(Same grade name, different standards)