Grade 17B2
Germany W-Nr. 1.5502
Corresponding Standard DIN EN 10263-4-2018
Steel rod, bars and wire for cold heading and cold extrusion Part 4: Technical delivery conditions for steels for quenching and tempering
Classification Alloy Steel
17B2 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Cu B
Minimum Value 0.15 - 0.6 - - - - 0.0008
Maximum Value 0.2 0.3 0.9 0.025 0.025 0.3 0.25 0.005
17B2 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Reduction of Area
ψ
%
Bar, rod, wire; 5<d≤25 Untreated or Pickling (+U or +PE) ≤540 ≥60
Bar, rod, wire; 5<d≤25 Spheroidizing or Spheroidizing and Peeling (+AC or +AC+PE) ≤460 ≥68
Wire; 5<d≤10 Untreated and Cold Drawn (+U+C) ≤630 ≥55
Wires; 10<d≤25 Untreated and Cold Drawn (+U+C) ≤620 ≥55
Wire; 2<d≤5 Unheated, Cold Drawn, and Spheroidized (+U+C+AC) ≤450 ≥70
Wire Rods; 5<d≤25 Unheated, Cold Drawn, and Spheroidized (+U+C+AC) ≤440 ≥70
Wire; 2<d≤5 Unheated, Cold Drawn, Spheroidized, and Quenched Rolling (+U+C+AC+LC) ≤490 ≥68
Wire Rods; 5<d≤25 Unheated, Cold Drawn, Spheroidized, and Quenched Rolling (+U+C+AC+LC) ≤480 ≥68
Wire; 5<d≤10 Spheroidizing + Cold Drawn (+AC+C) ≤550 ≥63
Wires; 10<d≤25 Spheroidizing + Cold Drawn (+AC+C) ≤540 ≥63
17B2 Corresponding Standards(Same grade name, different standards)