Grade
28B2
Germany W-Nr.
1.5510
Corresponding Standard
DIN EN 10263-4-2018
Steel rod, bars and wire for cold heading and cold extrusion Part 4: Technical delivery conditions for steels for quenching and tempering
Classification
Alloy Steel
28B2 Chemical Element Composition Content (%)
Component
C
Si ⓔ
Mn
P
S
Cr ⓕ
Cu
B
Minimum Value
0.25
-
0.6
-
-
-
-
0.0008
Maximum Value
0.3
0.3
0.9
0.025
0.025
0.3
0.25
0.005
28B2 Mechanical Properties
condition
Heat Treatment or Condition
Tensile Strength σb
Mpa
Reduction of Area ψ
%
Bar, rod, wire; 5<d≤25
Untreated or Pickling (+U or +PE)
≤630
≥60
Bar, rod, wire; 5<d≤25
Spheroidizing or Spheroidizing and Peeling (+AC or +AC+PE)
≤520
≥64
Wire; 5<d≤10
Untreated and Cold Drawn (+U+C)
≤720
≥55
Wires; 10<d≤25
Untreated and Cold Drawn (+U+C)
≤710
≥55
Wire; 2<d≤5
Unheated, Cold Drawn, and Spheroidized (+U+C+AC)
≤510
≥66
Wire Rods; 5<d≤25
Unheated, Cold Drawn, and Spheroidized (+U+C+AC)
≤500
≥66
Wire; 2<d≤5
Unheated, Cold Drawn, Spheroidized, and Quenched Rolling (+U+C+AC+LC)
≤550
≥64
Wire Rods; 5<d≤25
Unheated, Cold Drawn, Spheroidized, and Quenched Rolling (+U+C+AC+LC)
≤540
≥64
Wire; 5<d≤10
Spheroidizing + Cold Drawn (+AC+C)
≤610
≥59
Wires; 10<d≤25
Spheroidizing + Cold Drawn (+AC+C)
≤600
≥59
Approximate Comparison Table structural alloy steel
Germany
European Standard
DIN EN/DIN
EN
Numerical Grade
28B2
28B2
1.5510
28B2 Corresponding Standards(Same grade name, different standards)
Message
I want to correct it
Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!