Grade
32CrB4
Germany W-Nr.
1.7076
Corresponding Standard
DIN EN 10263-4-2018
Steel rod, bars and wire for cold heading and cold extrusion Part 4: Technical delivery conditions for steels for quenching and tempering
Classification
Alloy Steel
32CrB4 Chemical Element Composition Content (%)
Component
C
Si ⓔ
Mn
P
S
Cr ⓕ
Cu
B
Minimum Value
0.3
-
0.6
-
-
0.9
-
0.0008
Maximum Value
0.34
0.3
0.9
0.025
0.025
1.2
0.25
0.005
32CrB4 Mechanical Properties
condition
Heat Treatment or Condition
Tensile Strength σb
Mpa
Reduction of Area ψ
%
Bars, rods, wires; 5<d≤40
Spheroidizing or Spheroidizing and Peeling (+AC or +AC+PE)
≤550
≥62
Wire; 2<d≤5
Unheated, Cold Drawn, and Spheroidized (+U+C+AC)
≤550
≥64
Wire; 5<d≤40
Unheated, Cold Drawn, and Spheroidized (+U+C+AC)
≤530
≥64
Wire; 2<d≤5
Unheated, Cold Drawn, Spheroidized, and Quenched Rolling (+U+C+AC+LC)
≤590
≥62
Wire; 5<d≤40
Unheated, Cold Drawn, Spheroidized, and Quenched Rolling (+U+C+AC+LC)
≤570
≥62
Wire; 5<d≤40
Spheroidizing + Cold Drawn (+AC+C)
≤670
≥57
32CrB4 Corresponding Standards(Same grade name, different standards)
Message
I want to correct it
Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!