Grade X 6 CrNiTi 18 10
Corresponding Standard ISO 9329-4-1997
Austenitic stainless steels
Classification Austenitic Stainless Steel
X 6 CrNiTi 18 10 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni More
Minimum Value - - - - - 17 9 Ti≥5C≤0.80
Maximum Value 0.08 1 2 0.04 0.03 19 12
X 6 CrNiTi 18 10 Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
t ≤ 50, longitudinal Quenching, 1020~1120℃, Water Quenching, Air Cooling 490~690 40 ≥85
t ≤ 50, transverse Quenching, 1020~1120℃, Water Quenching, Air Cooling 490~690 35 ≥55
X6CrNiTi1810 Corresponding Standards(Same grade name, different standards)