Grade
C45RC
European Standard Steel Grade
1.1061
Corresponding Standard
EN 10263-4-2017
Steel Rod, Bars and Wire For Cold Heading and Cold Extrusion Part 4: Technical Delivery Conditions for Steels for Quenching and Tempering
Classification
Carbon Steel
Properties
Forgability
C45RC Chemical Element Composition Content (%)
Component
C ⓓ
Si ⓔ
Mn
P
S
Cu
Minimum Value
0.42
-
0.5
-
0.02
-
Maximum Value
0.5
0.3
0.8
0.025
0.035
0.25
C45RC Mechanical Properties
condition
Heat Treatment or Condition
Tensile Strength σb
Mpa
Reduction of Area ψ
%
Bars, wires; 2<d≤5
Untreated, Cold Drawn, Spheroidizing Treatment (+U+C+AC)
≤590
≥62
Bars, wires; 5<d≤40
Untreated, Cold Drawn, Spheroidizing Treatment (+U+C+AC)
≤580
≥62
Bars, wires; 2<d≤5
Untreated and Cold Drawn and Spheroidizing Treatment and Quenching Rolling (+U+C+AC+LC)
≤630
≥60
Bars, wires; 5<d≤40
Untreated and Cold Drawn and Spheroidizing Treatment and Quenching Rolling (+U+C+AC+LC)
≤620
≥60
Bar stock, rod stock; 5<d≤40
Spheroidizing or Spheroidizing + Rotary Peeling (+AC or +AC+PE)
≤600
≥60
Bar, Wire; 5<d≤10
Spheroidizing Treatment and Cold Drawing (+AC+C)
≤720
Bar, Wire; 10<d≤40
Spheroidizing Treatment and Cold Drawing (+AC+C)
≤710
Approximate Comparison Table Steel for Cold Heading and Cold Extrusion
International Organization for Standardization
European Standard
ISO
EN
Numerical Grade
C45RC
C45RC
1.1061
C45RC Corresponding Standards(Same grade name, different standards)
Message
I want to correct it
Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!