Grade
25CrMo4
European Standard Steel Grade
1.7218
Corresponding Standard
EN 10263-4-2017
Steel rod, bars and wire for cold heading and cold extrusion Part 4: Technical delivery conditions for steels for quenching and tempering
Classification
Alloy Steel
25CrMo4 Chemical Element Composition Content (%)
Component
C ⓓ
Si ⓔ
Mn
P
S
Cr
Cu
Mo
Minimum Value
0.22
-
0.6
-
-
0.9
-
0.15
Maximum Value
0.29
0.3
0.9
0.025
0.025
1.2
0.25
0.3
25CrMo4 Mechanical Properties
condition
Heat Treatment or Condition
Tensile Strength σb
Mpa
Reduction of Area ψ
%
Wire; 2<d≤5
Spheroidizing + Cold Drawn + Spheroidizing (+AC+C+AC)
≤570
≥62
Wire; 5<d≤40
Spheroidizing + Cold Drawn + Spheroidizing (+AC+C+AC)
≤560
≥62
Bars, wires; 2<d≤5
Spheroidizing + Cold Drawn + Spheroidizing + Quenched Rolling (+AC+C+AC+LC)
≤610
≥60
Bars, wires; 5<d≤40
Spheroidizing + Cold Drawn + Spheroidizing + Quenched Rolling (+AC+C+AC+LC)
≤600
≥60
Bars, rods, wires; 5<d≤40
Spheroidizing or Spheroidizing + Rotary Peeling (+AC or +AC+PE)
≤580
≥60
1 Approximate Comparison Table structural alloy steel
2 Approximate Comparison Table
3 Approximate Comparison Table
4 Approximate Comparison Table structural alloy steel
5 Approximate Comparison Table
Japan
International Organization for Standardization
European Standard
JIS
ISO
EN
Numerical Grade
SCM425
SCM425H
25CrMo4
25CrMo4
1.7218
25CrMo4 Corresponding Standards(Same grade name, different standards)
Message
I want to correct it
Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!