Grade
42CrMoS 4
European Standard Steel Grade
1.7227
Corresponding Standard
EN 10263-4-2017
Steel Rod, Bars and Wire For Cold Heading and Cold Extrusion Part 4: Technical Delivery Conditions for Steels for Quenching and Tempering
Classification
Alloy Steel
42CrMoS 4 Chemical Element Composition Content (%)
Component
C ⓓ
Si ⓔ
Mn
P
S
Cr
Cu
Mo
Minimum Value
0.38
-
0.6
-
0.02
0.9
-
0.15
Maximum Value
0.45
0.3
0.9
0.025
0.04
1.2
0.25
0.3
42CrMoS 4 Mechanical Properties
condition
Heat Treatment or Condition
Tensile Strength σb
Mpa
Reduction of Area ψ
%
Wire; 2<d≤5
Spheroidizing + Cold Drawn + Spheroidizing (+AC+C+AC)
≤620
≥60
Wire; 5<d≤40
Spheroidizing + Cold Drawn + Spheroidizing (+AC+C+AC)
≤610
≥60
Bars, wires; 2<d≤5
Spheroidizing + Cold Drawn + Spheroidizing + Quenched Rolling (+AC+C+AC+LC)
≤660
≥58
Bars, wires; 5<d≤40
Spheroidizing + Cold Drawn + Spheroidizing + Quenched Rolling (+AC+C+AC+LC)
≤650
≥58
Bars, rods, wires; 5<d≤40
Spheroidizing or Spheroidizing + Rotary Peeling (+AC or +AC+PE)
≤630
≥58
1 Approximate Comparison Table Alloy Steel for Quenching and Tempering
2 Approximate Comparison Table Steel for Cold Heading and Cold Extrusion
International Organization for Standardization
European Standard
ISO
EN
Numerical Grade
42CrMoS4
42CrMoS4
1.7227
42CrMoS4 Corresponding Standards(Same grade name, different standards)
Message
I want to correct it
Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!