Grade 17MnB4
European Standard Steel Grade 1.5520
Corresponding Standard EN 10263-4-2017
Steel rod, bars and wire for cold heading and cold extrusion Part 4: Technical delivery conditions for steels for quenching and tempering
Classification Alloy Steel
17MnB4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Cu B
Minimum Value 0.15 - 0.9 - - - - 0.0008
Maximum Value 0.2 0.3 1.2 0.025 0.025 0.3 0.25 0.005
17MnB4 Mechanical Properties
condtition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Reduction of Area
ψ
%
Bar, rod, wire; 5<d≤25 Untreated or Pickling (+U or +PE) ≤570 ≥60
Bar, rod, wire; 5<d≤25 Spheroidizing or Spheroidizing and Peeling (+AC or +AC+PE) ≤480 ≥67
Wire; 5<d≤10 Untreated and Cold Drawn (+U+C) ≤660 ≥55
Wires; 10<d≤25 Untreated and Cold Drawn (+U+C) ≤650 ≥55
Wire; 2<d≤5 Unheated, Cold Drawn, and Spheroidized (+U+C+AC) ≤470 ≥69
Wire Rods; 5<d≤25 Unheated, Cold Drawn, and Spheroidized (+U+C+AC) ≤460 ≥69
Wire; 2<d≤5 Unheated, Cold Drawn, Spheroidized, and Quenched Rolling (+U+C+AC+LC) ≤510 ≥67
Wire Rods; 5<d≤25 Unheated, Cold Drawn, Spheroidized, and Quenched Rolling (+U+C+AC+LC) ≤500 ≥67
Wire; 5<d≤10 Spheroidizing + Cold Drawn (+AC+C) ≤570 ≥62
Wires; 10<d≤25 Spheroidizing + Cold Drawn (+AC+C) ≤560 ≥62
1 Approximate Comparison Table
China Japan European Standard
GB ISC JIS EN
ML15MnB
GB/T 6478-2015
GB/T 6478-2001
A71154 SWRCHB 620
JIS G3508-1
17MnB4
EN 10263-4-2001
2 Approximate Comparison Table
International Organization for Standardization European Standard
ISO EN Numerical Grade
17 MnB4 17 MnB4 1.5520
17MnB4 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!