Grade
23MnB4
European Standard Steel Grade
1.5535
Corresponding Standard
EN 10263-4-2017
Steel Rod, Bars and Wire For Cold Heading and Cold Extrusion Part 4: Technical Delivery Conditions for Steels for Quenching and Tempering
Classification
Alloy Steel
23MnB4 Chemical Element Composition Content (%)
Component
C
Si ⓔ
Mn
P
S
Cr ⓕ
Cu
B
Minimum Value
0.2
-
0.9
-
-
-
-
0.0008
Maximum Value
0.25
0.3
1.2
0.025
0.025
0.3
0.25
0.005
23MnB4 Mechanical Properties
condition
Heat Treatment or Condition
Tensile Strength σb
Mpa
Reduction of Area ψ
%
Bar, rod, wire; 5<d≤25
Untreated or Pickling (+U or +PE)
≤600
≥60
Bar, rod, wire; 5<d≤25
Spheroidizing or Spheroidizing and Peeling (+AC or +AC+PE)
≤520
≥64
Wire; 5<d≤10
Untreated and Cold Drawn (+U+C)
≤700
≥55
Wires; 10<d≤25
Untreated and Cold Drawn (+U+C)
≤690
≥55
Wire; 2<d≤5
Unheated, Cold Drawn, and Spheroidized (+U+C+AC)
≤510
≥66
Wire Rods; 5<d≤25
Unheated, Cold Drawn, and Spheroidized (+U+C+AC)
≤500
≥66
Wire; 2<d≤5
Unheated, Cold Drawn, Spheroidized, and Quenched Rolling (+U+C+AC+LC)
≤550
≥64
Wire Rods; 5<d≤25
Unheated, Cold Drawn, Spheroidized, and Quenched Rolling (+U+C+AC+LC)
≤540
≥64
Wire; 5<d≤10
Spheroidizing + Cold Drawn (+AC+C)
≤620
≥59
Wires; 10<d≤25
Spheroidizing + Cold Drawn (+AC+C)
≤610
≥59
1 Approximate Comparison Table Steel for Cold Heading and Cold Extrusion
2 Approximate Comparison Table Steel for Cold Heading and Cold Extrusion
International Organization for Standardization
European Standard
ISO
EN
Numerical Grade
23 MnB4
23 MnB4
1.5535
23MnB4 Corresponding Standards(Same grade name, different standards)
Message
I want to correct it
Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!