Grade 36MnB4
European Standard Steel Grade 1.5537
Corresponding Standard EN 10263-4-2017
Steel rod, bars and wire for cold heading and cold extrusion Part 4: Technical delivery conditions for steels for quenching and tempering
Classification Alloy Steel
36MnB4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Cu B
Minimum Value 0.33 - 0.8 - - - - 0.0008
Maximum Value 0.38 0.3 1.1 0.025 0.025 0.3 0.25 0.005
36MnB4 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Reduction of Area
ψ
%
Bars, rods, wires; 5<d≤40 Spheroidizing or Spheroidizing and Peeling (+AC or +AC+PE) ≤600 ≥62
Wire; 2<d≤5 Unheated, Cold Drawn, and Spheroidized (+U+C+AC) ≤590 ≥64
Wire; 5<d≤40 Unheated, Cold Drawn, and Spheroidized (+U+C+AC) ≤580 ≥64
Wire; 2<d≤5 Unheated, Cold Drawn, Spheroidized, and Quenched Rolling (+U+C+AC+LC) ≤630 ≥62
Wire; 5<d≤40 Unheated, Cold Drawn, Spheroidized, and Quenched Rolling (+U+C+AC+LC) ≤620 ≥62
Wire; 5<d≤40 Spheroidizing + Cold Drawn (+AC+C) ≤700 ≥57
Approximate Comparison Table Steel for Cold Heading and Cold Extrusion
International Organization for Standardization European Standard
ISO EN Numerical Grade
36MnB4 36MnB4 1.5537
36MnB4 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!