Grade 37MnB5
European Standard Steel Grade 1.5538
Corresponding Standard EN 10263-4-2017
Steel rod, bars and wire for cold heading and cold extrusion Part 4: Technical delivery conditions for steels for quenching and tempering
Classification Alloy Steel
37MnB5 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Cu B
Minimum Value 0.35 - 1.15 - - - - 0.0008
Maximum Value 0.4 0.3 1.45 0.025 0.025 0.3 0.25 0.005
37MnB5 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Reduction of Area
ψ
%
Bars, rods, wires; 5<d≤40 Spheroidizing or Spheroidizing and Peeling (+AC or +AC+PE) ≤620 ≥62
Wire; 2<d≤5 Unheated, Cold Drawn, and Spheroidized (+U+C+AC) ≤610 ≥64
Wire; 5<d≤40 Unheated, Cold Drawn, and Spheroidized (+U+C+AC) ≤600 ≥64
Wire; 2<d≤5 Unheated, Cold Drawn, Spheroidized, and Quenched Rolling (+U+C+AC+LC) ≤650 ≥62
Wire; 5<d≤40 Unheated, Cold Drawn, Spheroidized, and Quenched Rolling (+U+C+AC+LC) ≤640 ≥62
Wire; 5<d≤40 Spheroidizing + Cold Drawn (+AC+C) ≤720 ≥57
1 Approximate Comparison Table Steel for Cold Heading and Cold Extrusion
China Japan International Organization for Standardization European Standard
GB ISC JIS ISO EN
ML35MnB
GB/T 6478-2015
GB/T 6478-2001
A71354 SWRCHB 734
JIS G3508.1-2010
35MnB5E
ISO 4954-1993
37MnB5
EN 10263-4-2001
2 Approximate Comparison Table Steel for Cold Heading and Cold Extrusion
International Organization for Standardization European Standard
ISO EN Numerical Grade
37MnB5 37MnB5 1.5538
37MnB5 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!