Grade SUS405-HR
Corresponding Standard JIS G 4311-2019
Heat-Resisting Steel Bars and Wire Rods
Classification Ferritic Stainless Steel
Properties Corrosion Resistance
Density 7.75 g/cm3
SUS405-HR Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Al
Minimum Value - - - - - 11.5 - 0.1
Maximum Value 0.08 1 1 0.04 0.03 14.5 0.6 0.3
SUS405-HR Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Annealing ≥410 ≥175 ≥20 ≥60 ≤183
SUS405-HR Corresponding Standards(Same grade name, different standards)