Grade 201LN
USA UNS S20153
Corresponding Standard ASTM A959-2019
Specifying Harmonized Standard Grade Compositions for Wrought Stainless Steels
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
201LN Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu N
Minimum Value - - 6.4 - - 16 4 - 0.1
Maximum Value 0.03 1 7.5 0.045 0.015 17.5 5 1 0.25
• Unless otherwise indicated, a grade designation originally assigned by the American Iron and Steel Institute (AISI).
Approximate Comparison Table Austenitic Stainless Steel
United States International Organization for Standardization European Standard
ASTM UNS ISO EN Numerical Grade
201LN S20153 X2CrMnNiN17-7-5 X2CrMnNiN17-7-5 1.4371
201LN Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!