Grade 32CrS2
Germany W-Nr. 1.7021
Corresponding Standard DIN 17200-1987
Steels for Quenching and Tempering; Technical Delivery Conditions
Classification Alloy Steel
32CrS2 Chemical Element Composition Content (%)
Component C Si Mn P S Cr
Minimum Value 0.28 - 0.5 - 0.02 0.4
Maximum Value 0.35 0.4 0.8 0.035 0.035 0.6
32CrS2 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
All Sizes Shearable condition (C) ≤255
All Sizes Softening Annealing (G) ≤197
d≤16 Quenching and Tempering (V) 700~850 ≥450 ≥15 ≥40 ISO-V
≥35
16<d≤40 Quenching and Tempering (V) 600~750 ≥350 ≥15 ≥45 ≥35
40<d≤100 Quenching and Tempering (V) 500~650 ≥300 ≥17 ≥50 ≥35

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!