Grade C25
Corresponding Standard DIN EN ISO 683-1-2018
Heat-treatable steels,alloy steels and free-cutting steels--Part 1: Non-alloy steels for quenching and tempering
Classification Carbon Steel
C25 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu Mo More
Minimum Value 0.22 0.1 0.4 - - - - - - Cr+Mo+Ni≤0.63
Maximum Value 0.29 0.4 0.7 0.045 0.045 0.4 0.4 0.3 0.1
C25 Mechanical Properties
Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
d≤16; t≤8 Quenching and Tempering 550~700 ≥370 ≥19
16<d≤40;8<t≤20 Quenching and Tempering 500~650 ≥320 ≥21
d≤16;t≤16 Normalizing (N) ≥470 ≥260 ≥22
16<d≤100;16<t≤100 Normalizing (N) ≥440 ≥230 ≥23
New and Old Grade Replacement List
Corresponding Standard Grade
DIN 17200-1987
Grade
Germany W-Nr.
DIN EN ISO 683-1-2018
Grade
1 Approximate Comparison Table
International Organization for Standardization Germany European Standard Russia
ISO DIN EN/DIN EN Numerical Grade GOST
C25 C25 C25 1.0406 25
2 Approximate Comparison Table
United States Germany France
ASTM/AISI DIN EN/DIN W-Nr. NF EN/NF
1025 C25 1.0406 CC28
C25 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!