Grade 20Cr4
Germany W-Nr. 1.7027
Corresponding Standard DIN 17210-1986
Case hardening steel coil
Classification Alloy Steel
Properties Carburizing Ability
20Cr4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr
Minimum Value 0.17 - 0.6 - - 0.9
Maximum Value 0.23 0.4 0.9 0.035 0.035 1.2
20Cr4 Mechanical Properties
condition Heat Treatment or Condition
Hardness
HBW
All product shapes Softening Annealing (G) ≤197
Bars, wire, plates, forgings; d≤150 Processed to a Certain Strength (BF) 149~197
Bar stock, plate, forgings; d≤60 Processed to Ferrite-Perlite Structure (BG) 145~192
1 Approximate Comparison Table structural alloy steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia United Kingdom
GB ISC CNS JIS KS ASTM/AISI UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST BS EN/BS
20Cr
20CrH
A20202 SCr420 SCr420
SCr420H
SCR420HRCH
SCr420 5120 G51200 20Cr4 20Cr4 1.7027 18C3 20Cr4 1.7027 20Х 527A20
2 Approximate Comparison Table
China Japan South Korea United States International Organization for Standardization Germany France Russia United Kingdom
GB ISC JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF GOST BS EN/BS
20CrH A20205 ≈SCr420H ≈SCr420H 5120H H51200 ≈20Cr4H 20Cr4 1.7027 (20MC5) 20Х (527H17)
3 Approximate Comparison Table
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany Russia
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. GOST
20Cr1H A20215 SCr420H SCr420H SCr420H ≈5120H ≈H51200 20Cr4H ≈20Cr4 ≈1.7027 20Х

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!