Grade X2CrNi12
Corresponding Standard ISO 9328-7-2018
Steel flat products for pressure purposes - Technical delivery conditions - Stainless steels
Classification Ferritic Stainless Steel
X2CrNi12 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni N
Minimum Value - - - - - 10.5 0.3 -
Maximum Value 0.03 1 1.5 0.04 0.015 12.5 1.1 0.03
X2CrNi12 Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
t≤8, Cold Rolled Steel Strips 450~650 ≥320 ≥20
t≤13.5, Hot Rolled Steel Strips 450~650 ≥320 ≥20
t≤25, Hot Rolled Steel Plate 450~650 ≥280 ≥18
1 Approximate Comparison Table
China United States International Organization for Standardization European Standard
GB ISC UNS ISO Numerical Grade EN Numerical Grade
022Cr12Ni S11213 S41003 X2CrNi12 4003-410-77-I X2CrNi12 1.4003
2 Approximate Comparison Table
China United States International Organization for Standardization European Standard
GB ISC UNS ISO Numerical Grade EN Numerical Grade
022Cr12Ni
GB/T 20878-2024
S11213 S40977
ASTM A959
X2CrNi12
ISO 15510
4003-410-77-I X2CrNi12
EN 10088-1
1.4003

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!