Grade 15NiCr13
Corresponding Standard DIN EN ISO 683-3-2019
Heat-treatable steels,alloy steels and free-cutting steels--Part 3: Case-hardening steels
Classification Alloy Steel
Properties Carburizing Ability
15NiCr13 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Cu
Minimum Value 0.12 0.15 0.35 - - 0.6 3 -
Maximum Value 0.18 0.4 0.65 0.025 0.035 0.9 3.5 0.4
15NiCr13 Mechanical Properties
condition Heat Treatment or Condition
Hardness
HBW
Semifinished products, bars Processed to a Certain Shearability (+S) ≤255
All product shapes Soft Annealing (+A) ≤229
Bar, wire, flat steel, forging Processed to a Certain Hardness (+TH) 179~229
Bar, forging Processed to Ferrite-Perlite Structure (+FP) 166~217
New and Old Grade Replacement List
Corresponding Standard Grade
DIN EN 10084-2008
Grade
Germany W-Nr.
DIN EN ISO 683-3-2019
Grade
Approximate Comparison Table Hardenability Guaranteed Structural Steel
China Taiwan, China Japan South Korea International Organization for Standardization Germany Russia
GB ISC CNS JIS KS ISO DIN EN/DIN W-Nr. GOST
20CrNi3H A42205 SNC631H SNC631H SNC631H ≈15NiCr3H ≈15NiCr13 ≈1.5752 20ХН3