Grade 17NiCrMoS6-4
Germany W-Nr. 1.6569
Corresponding Standard DIN EN 10084-2008
Case Hardening Steels – Technical Delivery Conditions
Classification Alloy Steel
17NiCrMoS6-4 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo
Minimum Value 0.14 - 0.6 - 0.02 0.8 1.2 0.15
Maximum Value 0.2 0.4 0.9 0.025 0.04 1.1 1.5 0.25
17NiCrMoS6-4 Mechanical Properties
condition Heat Treatment or Condition
Hardness
HBW
Semifinished products, bars Processed to a Certain Shearability (+S) ≤255
All product shapes Soft Annealing (+A) ≤229
Bar, wire, flat steel, forging Processed to a Certain Hardness (+TH) 179~229
Bar, forging Processed to Ferrite-Perlite Structure (+FP) 149~201
17NiCrMoS6-4 Corresponding Standards(Same grade name, different standards)