Grade X6CrNi23-13
Corresponding Standard ISO 9328-7-2018
Steel Flat Products for Pressure Purposes - Technical Delivery Conditions - Stainless Steels
Classification Austenitic Stainless Steel
X6CrNi23-13 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni N
Minimum Value 0.04 - - - - 22 12 -
Maximum Value 0.08 0.7 2 0.035 0.015 24 15 0.1
X6CrNi23-13 Mechanical Properties
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Impact Energy Absorption
KV2
J
t≤8, Cold Rolled Steel Strips 530~730 ≥220 ≥35 ≥100
t≤13.5, Hot Rolled Steel Strips 510~710 ≥200 ≥35 ≥100
t≤75, Hot rolled steel plates 510~710 ≥200 ≥35 ≥100
Approximate Comparison Table Austenitic Stainless Steel
China Taiwan, China Japan South Korea United States International Organization for Standardization Germany France European Standard Russia
GB ISC CNS JIS KS ASTM UNS ISO DIN EN/DIN W-Nr. NF EN/NF EN Numerical Grade GOST
06Cr23Ni13
(0Cr23Ni13)
S30908 309S SUS 309S STS 309S 309S S30908 X12CrNi 23-13
X6CrNi23-13
X7CrNi 23-14 1.4833 Z15CN 24-13 X12CrNi 23-13
X6CrNi23-13
1.4833
1.4950
10Х23Н13

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!