Grade X2CrNiMoN17-13-5
European Standard Steel Grade 1.4439
Corresponding Standard EN 10088-3-2014
Stainless steels-Part 3: Technical delivery condition for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes
Classification Austenitic Stainless Steel
Properties Corrosion Resistance
X2CrNiMoN17-13-5 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Ni Mo N
Minimum Value - - - - - 16.5 12.5 4 0.12
Maximum Value 0.03 1 2 0.045 0.015 18.5 14.5 5 0.22
X2CrNiMoN17-13-5 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
Bar, rod, wire, section, bright products; d≤160 +AT 580~800 ≥280 (long.)
≥35
≤250 (long.)
≥100
Bar, rod, wire, section, bright products; 160<d≤250 +AT 580~800 ≥280 (tr.)
≥30
≤250 (tr.)
≥60
1 Approximate Comparison Table
China United States International Organization for Standardization European Standard
GB ISC AISI UNS ISO Numerical Grade EN Numerical Grade
022Cr19Ni16Mo5N S31723 317LMN S31726 X2CrNiMoN17-13-5
X2CrNiMoN 18-15-5
4439-317-26-E
4483-317-26-I
X2CrNiMoN17-13-5 1.4439
(1.4483)
2 Approximate Comparison Table
United States France European Standard
ASTM UNS NF EN/NF EN Numerical Grade
317LMN S31726 Z3CND18-14-05Az X2CrNiMoN17-13-5 1.4439

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!