Grade X2CrNbCu21
European Standard Steel Grade 1.4621
Corresponding Standard EN 10088-3-2014
Stainless steels-Part 3: Technical delivery condition for semi-finished products, bars, rods, wire, sections and bright products of corrosion resisting steels for general purposes
Classification Ferritic Stainless Steel
Properties Corrosion Resistance
X2CrNbCu21 Chemical Element Composition Content (%)
Component C Si Mn P S Cr Cu N Al More
Minimum Value - - - - - 20 0.1 - - Nb:[7x(C+N)+0.1]~1.00
Maximum Value 0.03 1 1 0.04 0.015 21.5 1 0.03 0.5
X2CrNbCu21 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
Bar, rod, wire, section, bright products; d≤50 +A 420~640 ≥240 ≥20 ≤200
X2CrNbCu21 Corresponding Standards(Same grade name, different standards)

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!