Grade NiCr20TiAl
Germany W-Nr. 2.4952
Corresponding Standard DIN 17240-1976
Heat Resisting and Highly Heat Resisting Materials for Bolts and Nuts
Classification Nickel and Nickel Alloys
Properties Strength Corrosion Resistance High-Temperature Strength
Density 8.2 g/cm3
NiCr20TiAl Chemical Element Composition Content (%)
Component Fe C Si Mn P S Cr Ni Ti B Co Al
Minimum Value - - - - - - 18 65 1.8 - - 1
Maximum Value 3 0.1 1 1 0.03 0.015 21 - 2.7 0.008 2 1.8
NiCr20TiAl Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Impact Energy Absorption
KV2
J
d≤160 Precipitation Hardening (AH) ≥1000 ≥600 ≥12 ≥12 ISO-V
≥20
1 Approximate Comparison Table
China United States Germany France United Kingdom
GB ISC Commercial Grade DIN EN/DIN W-Nr. L-Nr. NF EN/NF BS EN/BS
GH4080A
(GH80A)
H40801 Nimonic 80A NiCr20TiAl 2.4952 2.4631 ATG S3
NC20TA
2HR1
2HR 201
2HR 401
3HR 601
DTD 736B
2 Approximate Comparison Table
China Japan United States Germany France Russia United Kingdom
GB JIS SAE W-Nr. L-Nr. NF EN/NF GOST Commercial Grade BS EN/BS
GH80A NCF80A HEV5 2.4952 2.4631 ATGS3
NC20TA
ЭИ445 ANC.9
N80A
DTD736B
HR1
HR201
HR401
HR601