Grade 35SMn20
Corresponding Standard DIN EN ISO 683-4-2018
Heat-treatable steels,alloy steels and free-cutting steels--Part 4: free-cutting steels
Classification Alloy Steel
Properties Machinability Quench Hardness
35SMn20 Chemical Element Composition Content (%)
Component C Si Mn P S
Minimum Value 0.32 - 0.9 - 0.15
Maximum Value 0.39 0.4 1.4 0.06 0.25
35SMn20 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
5<d≤10 Untreated (U) 580~770 ≤225
10<d≤16 Untreated (U) 580~770 ≤225
16<d≤40 Untreated (U) 560~750 ≤219
40<d≤63 Untreated (U) 560~740 ≤216
63<d≤100 Untreated (U) 550~740 ≤216
10<d≤16 Quenching and Tempering 620~820 ≥420 ≥14
16<d≤40 Quenching and Tempering 590~790 ≥365 ≥16
40<d≤63 Quenching and Tempering 540~740 ≥335 ≥17