Grade 38SMnPb28
Corresponding Standard DIN EN ISO 683-4-2018
Heat-treatable steels,alloy steels and free-cutting steels--Part 4: free-cutting steels
Classification Alloy Steel
Properties Machinability Quench Hardness
38SMnPb28 Chemical Element Composition Content (%)
Component C Si Mn P S Pb
Minimum Value 0.35 - 1.2 - 0.24 0.15
Maximum Value 0.4 0.4 1.5 0.06 0.33 0.35
38SMnPb28 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
5<d≤10 Untreated (U) 580~780 ≤228
10<d≤16 Untreated (U) 580~750 ≤219
16<d≤40 Untreated (U) 560~730 ≤213
40<d≤63 Untreated (U) 560~730 ≤213
63<d≤100 Untreated (U) 550~700 ≤204
5<d≤10 Quenching and Tempering 700~850 ≥480 ≥15
10<d≤16 Quenching and Tempering 700~850 ≥460 ≥15
16<d≤40 Quenching and Tempering 700~850 ≥420 ≥15
40<d≤63 Quenching and Tempering 700~850 ≥400 ≥16
63<d≤100 Quenching and Tempering 630~800 ≥380 ≥16