Grade 46S20
Corresponding Standard DIN EN ISO 683-4-2018
Heat-treatable steels,alloy steels and free-cutting steels--Part 4: free-cutting steels
Classification Alloy Steel
Properties Machinability Quench Hardness
46S20 Chemical Element Composition Content (%)
Component C Si Mn P S
Minimum Value 0.42 - 0.7 - 0.15
Maximum Value 0.5 0.4 1.1 0.06 0.25
46S20 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Hardness
HBW
5<d≤10 Untreated (U) 590~800 ≤234
10<d≤16 Untreated (U) 590~780 ≤228
16<d≤40 Untreated (U) 590~760 ≤222
40<d≤63 Untreated (U) 580~730 ≤213
63<d≤100 Untreated (U) 560~710 ≤207
5<d≤10 Quenching and Tempering 700~850 ≥490 ≥12
10<d≤16 Quenching and Tempering 700~850 ≥490 ≥12
16<d≤40 Quenching and Tempering 650~800 ≥430 ≥13
40<d≤63 Quenching and Tempering 630~780 ≥370 ≥14
63<d≤100 Quenching and Tempering 630~780 ≥370 ≥14
New and Old Grade Replacement List
Corresponding Standard Grade
DIN 1651-1988
Grade
Germany W-Nr.
DIN EN ISO 683-4-2018
Grade

Note: The data is for reference only! If you have any questions, please fill out "I want to correct it"!