Grade Cm30
Germany W-Nr. 1.1179
Corresponding Standard DIN 17200-1987
Classification Carbon Steel
Cm30 Chemical Element Composition Content (%)
Component C Si Mn P S
Minimum Value 0.27 - 0.5 - 0.02
Maximum Value 0.34 0.4 0.8 0.035 0.035
Cm30 Mechanical Properties
condition Heat Treatment or Condition
Tensile Strength
σb
Mpa
Yield Point
σs
Mpa
Elongation or Extension Rate
δ
%
Reduction of Area
ψ
%
Hardness
HBW
Impact Energy Absorption
KV2
J
Steel; All Sizes Softening Annealing (G) ≤170
Steel; d≤16 Quenching and Tempering (V) 600~750 ≥400 ≥18 ≥40 ISO-V
≥40
Steel; 16<d≤40 Quenching and Tempering (V) 550~700 ≥350 ≥20 ≥45 ≥40
Steel; 40<d≤100 Quenching and Tempering (V) 500~650 ≥300 ≥21 ≥50 ≥40
Flat steel; d≤16 Normalizing (N) 450~630 ≥280 Longitudinal
≥23
Flat steel; 16<d≤100 Normalizing (N) 450~630 ≥250 ≥23
Flat Steel; 100<d≤160 Normalizing (N) 430~610 ≥230 ≥21
New and Old Grade Replacement List
Corresponding Standard Grade
DIN 17200-1987
Grade
Germany W-Nr.
DIN EN ISO 683-1-2018
Grade